Printing in the network increase phenomenon is inevitable, but you can control.
Normally, coated fine print dot increases value must be less than 12%, general
printing quality to less than 18%, newspaper printing are controlled within 35%
(50% generally refers to the network). In the process of production, can
effectively control from the following several aspects.
1. Select
high-quality materials, reasonable control the exposure time and solution
concentration
Drying plate picture and text clear, network system, can
guarantee the network transfer effect, and can guarantee the plate have higher
resistance force. Usually to ensure that 5% of the dot is not lost, 95% of the
dot is not blurred.
2. Strictly control the printing ink in the balance
In
the process of printing, if water supply is too large, can lead to a layout for
the ink to increase, the ink layer thick, ink emulsification is severe, causing
imprinted dim without burnish. Boot in production process, in order to reduce
waste, usually in the boot will be increased to 150% of the normal water level,
after the normal printing, water should be gradually reduced to normal,
guaranteed by clear, saturated luster.
3. All kinds of printing pressure
control in a reasonable range
The plate cylinder and rubber roller pressure
control between 0.15 ~ 0.20 mm, and make sure that two parallel version of the
ink roller and the plate cylinder, under 100 mm in diameter on edition, ink
roller and printing plate cylinder pressure width is 3 ~ 4 mm in diameter 100 mm
or more depends on the version of the ink roller and printing plate cylinder
pressure width is 5 ~ 6 mm.
4. The correct version control run liquid
concentration
Education version liquid concentration control the balance of
ink and print quality plays vital role. Education version suitable concentration
of liquid can quickly rushed to locations around the "dirt". If education
version liquid concentration is low, dot around the ink cannot be removed, while
the increase lead to network, or lead to paste version; If education version
liquid concentration is too high, it will led to the decrease of the PS edition
print resistant force and education version of liquid waste. Usually run version
solution of pH control in 4.0 ~ 6.0, conductive value control in the 1400 us.
(Gold Printing Group)